| Refrigerant | Ozone Depletion Potential (ODP) | Global Warming Potential (GWP) |
| R-11 Trichlorofluoromethane | 1.0 | 4000 |
| R-12 Dichlorodifluoromethane | 1.0 | 2400 |
| R-13 B1 Bromotrifluoromethane | 10 | |
| R-22 Chlorodifluoromethane | 0.05 | 1700 |
| R-32 Difluoromethane | 0 | 650 |
| R-113 Trichlorotrifluoroethane | 0.8 | 4800 |
| R-114 Dichlorotetrafluoroethane | 1.0 | 3.9 |
| R-123 Dichlorotrifluoroethane | 0.02 | 0.02 |
| R-124 Chlorotetrafluoroethane | 0.02 | 620 |
| R-125 Pentafluoroethane | 0 | 3400 |
| R-134a Tetrafluoroethane | 0 | 1300 |
| R-143a Trifluoroethane | 0 | 4300 |
| R-152a Difluoroethane | 0 | 120 |
| R-245a Pentafluoropropane | 0 | |
| R-401A (53% R-22, 34% R-124, 13% R-152a) | 0.37 | 1100 |
| R-401B (61% R-22, 28% R-124, 11% R-152a) | 0.04 | 1200 |
| R-402A (38% R-22, 60% R-125, 2% R-290) | 0.02 | 2600 |
| R-404A (44% R-125, 52% R-143a, R-134a) | 0 | 3300 |
| R-407A (20% R-32, 40% R-125, 40% R-134a) | 0 | 2000 |
| R-407C (23% R-32, 25% R-125, 52% R-134a) | 0 | 1600 |
| R-502 (48.8% R-22, 51.2% R-115) | 0.283 | 4.1 |
| R-507 (45% R-125, 55% R-143) | 0 | 3300 |
| R-717 Ammonia - NH3 | 0 | 0 |
| R-718 Water - H20 | 0 | |
| R-729 Air | 0 | |
| R-744 Carbon Dioxide - CO2 | 1 |