Fluid Absolute Viscosity
(N s/m2, Pa s)
Acetic acid 0.00116
Acetone 0.00032
Alcohol, ethyl (ethanol) 0.0011
Alcohol, methyl (methanol) 0.00056
Alcohol, propyl 0.0019
Benzene 0.0006
Bromine 0.00095
Carbon Disulfide 0.00036
Carbon Tetrachloride 0.00091
Castor Oil 0.650
Chloroform 0.00053
Decane 0.00086
Dodecane 0.00137
Ether 0.00022
Ethylene Glycol 0.016
Freon refrigerant R-11 0.00042
Glycerine 0.950
Heptane 0.00038
Hexane 0.000297
Kerosene 0.0016
Linseed Oil 0.033
Mercury 0.0015
Octane 0.00051
Phenol 0.0080
Propane 0.00011
Propylene 0.00009
Propylene glycol 0.042
Toluene 0.00055
Turpentine 0.0014
Water, Fresh 0.00089