Designation Dimensions Static Parameters
Moment of Inertia Section Modulus
Imperial
(in x in)
Depth
h
(in)
With
w
(in)
Web Thickness
s
(in)
Sectional Area
(in2)
Weight
(lb/ft)
Ix
(in4)
Iy
(in4)
Wx
(in3)
Wy
(in3)
2 x 1 2 1 0.13 0.49 0.58 0.288 0.05 0.29 0.06
2 x 1 1/4 2 1 1/4 0.17 0.91 1.07 0.546 0.14 0.55 0.18
3 x 1 1/2 3 1 1/2 0.13 0.97 1.14 1.41 0.22 0.94 0.22
3 x 1 3/4 3 1 3/4 0.17 1.36 1.60 1.97 0.42 1.31 0.37
4 x 2 4 2 0.15 1.48 1.74 3.91 0.60 1.95 0.45
4 x 2 1/4 4 2 1/4 0.19 1.98 2.33 5.21 1.0 2.60 0.69
5 x 2 1/4 5 2 1/4 0.15 1.88 2.21 7.88 1.0 3.15 0.64
5 x 2 3/4 5 2 3/4 0.19 2.63 3.09 11.1 2.1 4.45 1.14
6 x 2 1/2 6 2 1/2 0.17 2.41 2.83 14.4 1.5 4.78 0.90
6 x 3 1/4 6 3 1/4 0.21 3.43 4.03 21.0 3.8 7.0 1.8
7 x 2 3/4 7 2 3/4 0.17 2.73 3.21 22.1 2.1 6.3 1.1
7 x 3 1/2 7 3 1/2 0.21 4.01 4.72 33.8 5.1 9.7 2.2
8 x 3 8 3 0.19 3.53 4.15 37.4 3.3 9.4 1.6
8 x 3 3/4 8 3 3/4 0.25 4.92 5.78 52.7 7.1 13.2 2.8
9 x 3 1/4 9 3 1/4 0.23 4.24 4.98 54.4 4.4 12.1 1.9
9 x 4 9 4 0.29 5.93 6.97 78.3 9.6 17.4 3.5
10 x 3 1/2 10 3 1/2 0.25 5.22 6.14 83.2 6.3 16.6 2.6
10 x 4 1/4 10 4 1/4 0.31 7.11 8.36 116.2 13.0 23.2 4.5
12 x 4 12 4 0.29 7.04 8.27 159.8 11.0 26.6 3.9
12 x 5 12 5 0.35 10.1 11.8 239.7 25.7 40.0 7.6