Properties  in imperial units of American Steel Channels are indicated below.

Designation Dimensions Static Parameters
Moment of Inertia Section Modulus
Imperial
(in x lb/ft)
Depth
h
(in)
With
w
(in)
Web Thickness
s
(in)
Sectional Area
(in2)
Weight
(lb/ft)
Ix
(in4)
Iy
(in4)
Wx
(in3)
Wy
(in3)
C 15 x 50 15 3.716 0.716 14.7 50 404 11.0 53.8 3.78
C 15 x 40 15 3.520 0.520 11.8 40 349 9.23 46.5 3.37
C 15 x 33.9 15 3.400 0.400 9.96 33.9 315 8.13 42.0 3.11
                   
C 12 x 30 12 3.170 0.510 8.82 30 162 5.14 27.0 2.06
C 12 x 25 12 3.047 0.387 7.35 25 144 4.47 24.1 1.88
C 12 x 20.7 12 2.942 0.282 6.09 20.7 129 3.88 21.5 1.73
                   
C 10 x 30 10 3.033 0.673 8.82 30 103 3.94 20.7 1.65
C 10 x 25 10 2.886 0.526 7.35 25 91.2 3.36 18.2 1.48
C 10 x 20 10 2.739 0.379 5.88 20 78.9 2.81 15.8 1.32
C 10 x 15.3 10 2.600 0.240 4.49 15.3 67.4 2.28 13.5 1.16
                   
C 9 x 20 9 2.648 0.448 5.88 20 60.9 2.42 13.5 1.17
C 9 x 15 9 2.485 0.285 4.41 15 51.0 1.93 11.3 1.01
C 9 x 13.4 9 2.433 0.233 3.94 13.4 47.9 1.76 10.6 0.96
                   
C 8 x 18.75 8 2.527 0.487 5.51 18.75 44.0 1.98 11.0 1.01
C 8 x 13.75 8 2.343 0.303 4.04 13.75 36.1 1.53 9.03 0.85
C 8 x 11.75 8 2.260 0.220 3.38 11.5 32.6 1.32 8.14 0.78
                   
C 7 x 14.75 7 2.299 0.419 4.33 14.75 27.2 1.38 7.78 0.78
C 7 x 12.25 7 2.194 0.314 3.60 12.25 24.2 1.17 6.93 0.70
C 7 x 9.8 7 2.090 0.210 2.87 9.8 21.3 0.97 6.08 0.63
                   
C 6 x 13 6 2.157 0.437 3.83 13 17.4 1.05 5.80 0.64
C 6 x 10.5 6 2.034 0.314 3.09 10.5 15.2 0.87 5.06 0.56
C 6 x 8.2 6 1.920 0.200 2.40 8.2 13.1 0.69 4.38 0.49
                   
C 5 x 9 5 1.885 0.325 2.64 9 8.90 0.63 3.56 0.45
C 5 x 6.7 5 1.750 0.190 1.97 6.7 7.49 0.48 3.00 0.38
                   
C 4 x 7.25 4 1.721 0.321 2.13 7.25 4.59 0.43 2.29 0.34
C 4 x 5.4 4 1.584 0.184 1.59 5.4 3.85 0.32 1.93 0.28
                   
C 3 x 6 3 1.596 0.356 1.76 6 2.07 0.31 1.38 0.27
C 3 x 5 3 1.498 0.258 1.47 5 1.85 0.25 1.24 0.23
C 3 x 4.1 3 1.410 0.170 1.21 4.1 1.66 0.20 1.10 0.20

The standard method for specifying the dimensions of a American Standard Steel Channels is like C 5 x 9. which is a beam 5 inches deep with a weight 9 lb/ft.

I-shaped cross-section beams: