Engineering ToolBox > Cross Reference of ASTM Material Specifications
A ASTM cross reference material specification of fittings, flanges, unions and cast and forged valves can be found in the table below:
| Material | Forgings | Castings | Wrought Fittings |
| Carbon Steel Cold Temperature Service | A105 A350-LF2 | A216-WCB | A234-WPB A420-WPL6 |
| Carbon-1/2 Molybdenum Alloy Steel High Temperature Service | A182-F1 | A217-WC1 A352-LC1 | A234-WP1 |
| 3-1/2 Nickel Alloy Steel Low Temperature Service | A350-LF3 | A352-LC3 | A420-WPL3 |
| 1/2 Cr-1/2 Mo Alloy Steel 1/2 Cr-1/2 Mo-1 Ni Alloy 3/4 Cr-1 Mo-3/4 Ni Alloy Steel 1 Cr-1/2 Mo Alloy Steel | A182-F2 A182-F12 CL2 | A217-WC4 A217-WC5 | A234-WP12 CL2 |
| 1-1/4 Cr-1/2 Mo Alloy Steel 2-1/4 Cr-1 Mo Alloy Steel 5 Cr-1/2 Mo Alloy Steel 5 Cr-1/2 Mo Alloy Steel 9 Cr-1 Mo Alloy Steel 13 Cr Alloy Steel | A182-F11 CL2 A182-F22 CL3 A182-F5 A182-F5a A182-F9 A182-F6 | A217-WC6 A217-WC9 A217-C5 A217-C12 A743-CA15 | A234-WP11 CL2 A234-WP22 CL3 A234-WP5 A234-WP9 |
| Type 304 Stainless Steel (18 Cr-8 Ni) Standard Low Carbon High Temperature Service | A182-F304 A182-F304L A182-F304H | A351-CF3 A351-CF8 | A403-WP304 A403-WP304L A403-WP304H |
| Type 310 Stainless Steel (25 Cr-20 Ni) Type 316 Stainless Steel (16 Cr-12 Ni-2 Mo) Standard Low Carbon High Temperature | A182-F310H A182-F316 A182-F316L A182-F316H | A351-CK20 A351-CF3M A351-CF8M | A403-WP310 A403-WP316 A403-WP316L A403-WP316H |
| Type 317 Stainless Steel (18 Cr-13 Ni-3 Mo) Type 321 Stainless Steel (18 Cr-10 Ni-Ti) Standard High Temperature Service | A182-F321 A182-F321H | A403-WP317 A403-WP321 A403-WP321H | |
| Type 347 Stainless Steel (18 Cr-10 Ni-Cb) Standard High Temperature Service | A182-F347 A182-F347H | A351-CF8C | A403-WP347 A403-WP347H |
| Type 348 Stainless Steel (18 Cr-10 Ni-Cb) Standard High Temperature Service | A182-F348 A182-F348H | A403-WP348 A403-WP438H |