Resources, Tools and Basic Information for Engineering and Design of Technical Applications!
mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!
Engineering ToolBox > Copper Tubes DWV - Drain, Waste and Vent
Copper tubes according ASTM 306 are used in soil, waste, vent, solar and storm drainage piping systems.
| Nominal Diameter (inches) | Outside Diameter (inches) | Inside Diameter (inches) | Wall Thickness (inches) | Cross Sectional Area of Bore (square inches) | Weight (lb/ft) | Weight with Water (lb/ft) |
| 1 1/4 | 1.375 | 1.295 | 0.040 | 1.32 | 0.650 | 1.22 |
| 1 1/2 | 1.625 | 1.541 | 0.042 | 1.87 | 0.809 | 1.62 |
| 2 | 2.125 | 2.041 | 0.042 | 3.27 | 1.07 | 2.48 |
| 3 | 3.125 | 3.030 | 0.045 | 7.21 | 1.69 | 4.81 |
| 4 | 4.125 | 4.009 | 0.058 | 11.6 | 2.87 | 7.88 |
| 5 | 5.125 | 4.981 | 0.072 | 19.5 | 4.43 | 12.9 |
| 6 | 6.125 | 5.959 | 0.083 | 27.9 | 6.10 | 18.2 |