Solid Density
(103 kg/m3) (lb/ft3)
ABS   66
Agate 2.5 - 2.6 156 - 168
Acrylic   74
Alabaster carbonate 2.7 - 2.8 168 - 173
Alabaster sulfate 2.3 143
Aluminium 2.7 167
Aluminum Bronze   486
Albite 2.6 - 2.65 163 - 165
Alloys    
Amber 1.06 - 1.1 66 - 69
Amphiboles 2.9 - 3.2 180 - 200
Anorthite 2.74 - 2.76 171 - 172
Arsenic 4.7 291
Asbestos 2.0 - 2.8 125 - 175
Asbestos slate 1.8 112
Asphalt 1.1 - 1.5 69 - 94
Basalt 2.4 - 3.1 150 - 190
Beeswax 0.96 60 - 61
Beryl 2.7 168
Biotite 2.7 - 3.1 170 - 190
Bismuth 9.8 607
Bone 1.7 - 2.0 106 - 125
Borax   112
Brick 1.4 - 2.2 87 - 137
Brick, fire   143
Brick, hard   125
Brick, pressed   137
Brickwork in cement   112
Brickwork in mortar   100
Butter 0.87 53
Calamine 4.1 - 4.5 255 - 280
Calcspar 2.6 - 2.8 162 - 175
Camphor 1 62
Caoutchouc 0.9 - 1 57 - 62
Cardboard 0.7 43
Celluloid 1.4 87
Cement, set 2.7 - 3 170 - 190
Chalk 1.9 - 2.8 118 - 175
Charcoal, oak 0.6 35
Charcoal, pine 0.3 - 0.4 18 - 28
Cinnabar 8.1 507
Clay 1.8 - 2.6 112 - 162
Coal, anthracite 1.4 - 1.8 87 - 112
Coal, bituminous 1.2 - 1.5 75 - 94
Cocoa, butter 0.9 56
Coke 1 - 1.7 62 - 105
Concrete    
Copal 1 - 1.15 65 - 71
Cork 0.2 - 0.25 14 - 16
Cork, linoleum 0.55 34
Corundum 4.0 247
CPVC   97
Lead Crystal 3.1 192
Diamond 3 - 3.5 188 - 220
Dolomite 2.8 177
Earth, loose   75
Earth, rammed   100
Ebonite 1.15 72
Emery 4 250
Epidote 3.2 - 3.5 203 - 218
Feldspar 2.6 - 2.8 159 - 172
Flint 2.6 164
Fluorite 3.2 198
Galena 7.3 - 7.6 460 - 470
Gallium 5.9 366
Gamboge 1.2 75
Garnet 3.2 - 4.3 197 - 268
Gas carbon 1.9 117
Gelatin 1.3 79
Germanium 5.32 330
Glass, common 2.4 - 2.8 150 - 175
Glass, flint 2.9 - 5.9 180 - 370
Glue 1.3 79
Granite 2.6 - 2.8 165 - 172
Graphite 2.3 - 2.7 144 - 170
Gum arabic 1.3 - 1.4 81 - 87
Gypsum 2.3 144
Hematite 4.9 - 5.3 306 - 330
Hornblende 3 187
Ice 0.917 57.2
Iron 7.87 488
Ivory 1.8 - 1.9 114 - 120
Leather, dry 1.3 - 1.4 54
Lime, slaked 1.35 84
Limestone 2.7 -2.8 167 - 171
Linoleum 1.2 74
Magnetite 4.9 - 5.2 306 - 324
Malachite 3.7 - 4.1 231 - 256
Marble 2.6 - 2.8 160 - 177
Meerschaum 1 - 1.3 62 - 80
Metals    
Mica 2.6 - 3.2 165 - 200
Muscovite 2.8 - 3 172 - 187
Ochre 3.5 218
Opal 2.2 137
Paper 0.7 - 1.15 44 - 72
Paraffin 0.9 55
Peat blocks 0.85 52
Pitch 1.1 67
Porcelain 2.3 - 2.5 143 - 156
Porphyry 2.6 - 2.9 162 - 181
Pressed wood, pulp board 0.19 12
Pyrite 4.9 - 5.1 309 - 318
Quartz 2.65 165
Resin 1.07 67
Rock salt 2.2 136
Rubber, hard 1.2 74
Rubber, soft commercial 1.1 69
Rubber, pure gum 0.91 - 0.93 57 - 58
Sandstone 2.1 - 2.4 134 - 147
Serpentine 2.5 - 2.65 156 - 165
Silica, fused transparent 2.2 138
Silica, translucent 2.1 129
Silicon 2.33 144
Slag 2 - 3.9 125 - 240
Slate 2.6 - 3.3 162 - 205
Soapstone 2.6 - 2.8 162 - 175
Spermaceti 0.95 59
Starch 1.5 95
Sugar 1.6 99
Talc 2.7 - 2.8 168 - 174
Tallow, beef 0.95 59
Tallow, mutton 0.95 59
Tar 1.05 66
Topaz 3.5 - 3.6 219 - 223
Tourmaline 3 - 3.2 190 - 200
Wax, sealing 1.8 112
Wood (seasoned)    