Storage Typical Energy Densities
(kJ/kg) (MJ/m3)
Thermal Energy, low temperature Water, temperature difference 100oC to 40oC 250 250
Stone or rocks, temperature difference 100oC to 40oC 40 - 50 100 - 150
Iron, temperature difference 100oC to 40oC 30 230
Thermal Energy, high temperature Stone or rocks, temperature difference 400oC to 200oC 160 430
Iron, temperature difference 400oC to 200oC 100 800
Conventional Fuels Energy Crude Oil 42 000 37 000
Coal 32 000 42 000
Dry Wood 12 500 - 20 000 10 000 - 16 000
Synthetic Fuels Energy Hydrogen, gas 120 000 10
Hydrogen, liquid 120 000 8 700
Methanol 21 000 17 000
Ethanol 28 000 22 000
Electrochemical Energy Lead-acid batteries 40 - 140 100 - 900
Nickel-cadmium batteries 350 350
Lithium ion batteries 700 1400
Mechanical Energy Hydropower, 100 m head 1 1
Compressed air   15
Flywheel, steel 30 - 120 240 - 950
Flywheel, composite materials > 200 > 100