Specific heat of Ethylene Gas - C2H4 - at temperatures ranging 175 - 900 K are indicated in the table below:
| Ethylene Gas - C2H4 | |
| Temperature - T - (K) |
Specific Heat - cp - (kJ/kg.K) |
| 175 | 1.241 |
| 200 | 1.260 |
| 225 | 1.316 |
| 250 | 1.380 |
| 275 | 1.453 |
| 300 | 1.535 |
| 325 | 1.621 |
| 350 | 1.709 |
| 375 | 1.799 |
| 400 | 1.891 |
| 450 | 2.063 |
| 500 | 2.227 |
| 550 | 2.378 |
| 600 | 2.519 |
| 650 | 2.649 |
| 700 | 2.770 |
| 750 | 2.883 |
| 800 | 2.989 |
| 850 | 3.088 |
| 900 | 3.180 |