| HEM | Dimensions | Static Parameters | |||||||
| Moment of Inertia | Section Modulus | ||||||||
| Depth h (mm) | Width w (mm) | Web Thickness s (mm) | Sectional Area (cm2) | Weight (kg/m) | Ix (cm4) | Iy (cm4) | Wx (cm3) | Wy (cm3) | |
| 100M | 120 | 106 | 12 | 53.2 | 41.8 | 1140 | 399 | 190 | 75.3 |
| 120M | 140 | 126 | 12.5 | 66.4 | 52.1 | 2020 | 703 | 288 | 112 |
| 140M | 160 | 146 | 13 | 80.6 | 63.2 | 3290 | 1140 | 411 | 157 |
| 160M | 180 | 166 | 14 | 97.1 | 76.2 | 5100 | 1760 | 566 | 212 |
| 180M | 200 | 186 | 14.5 | 113 | 88.9 | 7480 | 2580 | 748 | 277 |
| 200M | 220 | 206 | 15 | 131 | 103 | 10640 | 3650 | 967 | 354 |
| 220M | 240 | 226 | 15.5 | 149 | 117 | 14600 | 5010 | 1220 | 444 |
| 240M | 270 | 248 | 18 | 200 | 157 | 24290 | 8150 | 1800 | 657 |
| 260M | 290 | 268 | 18 | 220 | 172 | 31310 | 10450 | 2160 | 780 |
| 280M | 310 | 288 | 18.5 | 240 | 189 | 39550 | 13160 | 2550 | 914 |
| 300M | 340 | 310 | 21 | 303 | 238 | 59200 | 19400 | 3480 | 1250 |
| 320M | 359 | 309 | 21 | 312 | 245 | 68130 | 19710 | 3800 | 1280 |
| 340M | 377 | 309 | 21 | 316 | 248 | 76370 | 19710 | 4050 | 1280 |