| Designation | Dimensions | Static Parameters | |||||||
| Moment of Inertia | Section Modulus | ||||||||
| Depth h (mm) | Width w (mm) | Web Thickness s (mm) | Sectional Area (cm2) | Weight (kg/m) | Ix (cm4) | Iy (cm4) | Wx (cm3) | Wy (cm3) | |
| I 80 | 80 | 42 | 3,9 | 7,58 | 5,94 | 77,8 | 6,29 | 19,5 | 3 |
| I 100 | 100 | 50 | 4,5 | 10,6 | 8,34 | 171 | 12,2 | 34,2 | 4,88 |
| I 120 | 120 | 58 | 5,1 | 14,2 | 11,1 | 328 | 21,5 | 54,7 | 7,41 |
| I 140 | 140 | 66 | 5,7 | 18,3 | 14,3 | 573 | 35,2 | 81,9 | 10,7 |
| I 160 | 160 | 74 | 6,3 | 22,8 | 17,9 | 935 | 54,7 | 117 | 14,8 |
| I 180 | 180 | 82 | 6,9 | 27,9 | 21,9 | 1450 | 81,3 | 161 | 19,8 |
| I 200 | 200 | 90 | 7,5 | 33,5 | 26,2 | 2140 | 117 | 214 | 26 |
| I 220 | 220 | 98 | 8,1 | 39,6 | 31,1 | 3060 | 162 | 278 | 33,1 |
| I 240 | 240 | 106 | 8,7 | 46,1 | 36,2 | 4250 | 221 | 354 | 41,7 |
| I 260 | 260 | 113 | 9,4 | 53,4 | 41,9 | 5740 | 288 | 442 | 51 |
| I 300 | 300 | 125 | 10,8 | 69,1 | 54,2 | 9800 | 451 | 653 | 72,2 |
| I 340 | 340 | 137 | 12,2 | 86,8 | 68 | 15700 | 674 | 923 | 98,4 |
| I 360 | 360 | 143 | 13 | 97,1 | 76,1 | 19610 | 818 | 1090 | 114 |
| I 400 | 400 | 155 | 14,4 | 118 | 92,4 | 29210 | 1160 | 1460 | 149 |
| I 450 | 450 | 170 | 16,2 | 147 | 115 | 45850 | 1730 | 2040 | 203 |
| I 500 | 500 | 185 | 18 | 180 | 141 | 68740 | 2480 | 2750 | 268 |