| Temperature - t - (�C) | Density - ρ - (kg/m3) | Thermal Conductivity - k - (W/mK) | Specific Heat - cp - (kJ/kgK) |
| 0.01 (Water) | 999.8 | ||
| 0 | 916.2 | 2.22 | 2.050 |
| -5 | 917.5 | 2.25 | 2.027 |
| -10 | 918.9 | 2.30 | 2.000 |
| -15 | 919.4 | 2.34 | 1.972 |
| -20 | 919.4 | 2.39 | 1.943 |
| -25 | 919.6 | 2.45 | 1.913 |
| -30 | 920.0 | 2.50 | 1.882 |
| -35 | 920.4 | 2.57 | 1.851 |
| -40 | 920.8 | 2.63 | 1.818 |
| -50 | 921.6 | 2.76 | 1.751 |
| -60 | 922.4 | 2.90 | 1.681 |
| -70 | 923.3 | 3.05 | 1.609 |
| -80 | 924.1 | 3.19 | 1.536 |
| -90 | 924.9 | 3.34 | 1.463 |
| -100 | 925.7 | 3.48 | 1.389 |