Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!

Engineering ToolBox > Thermal Expansion - Linear

Linear temperature expansion - online calculator

Linear thermal expansion can be expressed as

dl = L0 α (t1 - t0) (1)

where

dl = change in length (m)

L0 = initial length (m)

α =  linear expansion coefficient

t0 = initial temperature (oC)

t1 = final temperature (oC)

Online Thermal Linear Expansion Calculator

L0 - initial length (m)

α - linear expansion coefficient

t0 - initial temperature (oC)

t1 - final temperature (oC)

Change in length (dL): (m)

Final length (L1): (m)

Linear Temperature Coefficients - α - of some common metals

 

Related Topics

Engineering Toolbox >

Related Documents

Google


Web The Engineering ToolBox
.