Melting and boiling temperatures, and latent heat of evaporation and melting heat from solid to fluid state of some common substances, can be found in the table below:
| Substance | Melting Point Temperature - t - (oC) | Latent Heat of Melting - Lf - (kJ/kg) | Boiling Point - Vaporization - Temperature - t - (oC) | Latent Heat of Evaporation - Lv - (kJ/kg) |
| Aluminum | 659 | 399 | 2,327 | 10,530 |
| Brass | 930 | |||
| Cobalt | 1480 | 2900 | ||
| Copper | 1,083 | 207 | 2,595 | 4,730 |
| Ethyl alcohol | 114 | 108 | 78.3 | 855 |
| Gold | 1,063 | 64 | 2,600 | 1,577 |
| Graphite | 3500 | |||
| Hydrogen | 259 | 58.0 | 253 | 455 |
| Lead | 328 | 23 | 1,750 | 859 |
| Manganese | 1260 | 2150 | ||
| Magnesium | 650 | 1110 | ||
| Mercury | 39 | 11 | 357 | 295 |
| Molybdenum | 2620 | 5560 | ||
| Nickel | 1455 | 2730 | ||
| Nitrogen | 210 | 25.7 | 196 | 200 |
| Oxygen | 219 | 13.9 | 183 | 213 |
| Silver | 962 | 111 | 1,950 | 2,356 |
| Titanium | 1700 | 3260 | ||
| Tungsten | 3370 | 5930 | ||
| Zinc | 420 | 906 | ||
| Water | 0 | 335 | 100 | 2,272 |