Resources, Tools and Basic Information for Engineering and Design of Technical Applications!
mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!
Engineering ToolBox > Melting and Solidifying Points
Melting and solidifying temperatures of some common products can be found in the table below:
| Product | Melting and Solidifying Temperature | |
| (oC) | (oF) | |
| Alcohol | -97 | -143 |
| Aluminum | 658 | 1,218 |
| Ammonia | -78 | -108 |
| Aniline | -6 | 21 |
| Carbon dioxide | -56 | -69 |
| Copper | 1,083 | 1,981 |
| Dowtherm | 12 | 54 |
| Glycerin | -16 | 4 |
| Gold | 1,063 | 1,945 |
| Iron, pure | 1,530 | 2,786 |
| Lead | 327 | 621 |
| Mercury | -39 | -38 |
| Nickel | 1,455 | 2,646 |
| Silver | 960 | 1,761 |
| Sulphur | 106 - 119 | 234 - 247 |
| Tin | 232 | 449 |
| Water | 0 | 32 |
| Wax | 64 | 149 |
| Zinc | 419 | 787 |