Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!

Engineering ToolBox > Metals and Alloys - Densities

Density of some common metals and alloys - aluminum, bronze, copper, iron and more

The density of some common metals and alloys can be found in the table below:

Metal or Alloy Density 
(kg/m3)
Admiralty Brass 8525
Aluminum 2712
Aluminum - melted 2560 - 2640
Aluminum bronze (3-10% Al) 7700 - 8700
Aluminum foil 2700 -2750
Antifriction metal 9130 -10600
Beryllium 1840
Beryllium copper 8100 - 8250
Brass - casting 8400 - 8700
Brass - rolled and drawn 8430 - 8730
Bronze - lead 7700 - 8700
Bronze - phosphorous 8780 - 8920
Bronze (8-14% Sn) 7400 - 8900
Cast iron 6800 - 7800
Chemical Lead 11340
Cobolt 8746
Copper 8930
Cupronickel 8940
Delta metal 8600
Electrum 8400 - 8900
Gold 19320
Hatelloy 9245
 Inconel 8497
Incoloy 8027
Iron 7850
Lead 11340
Light alloy based on Al 2560 - 2800
Light alloy based on Mg 1760 - 1870
Magnesium 1738
Manganese Bronze 8359
Mercury 13593
Molybdenum 10188
Monel 8360 - 8840
Nickel 8800
Nickel silver 8400 - 8900
Platinum 21400
Plutonium 19816
Red Brass 8746
Silver 10490
Solder 50/50 Pb Sn 8885
Stainless Steel  7480 - 8000
Steel 7850
Tin 7280
Titanium 4500
Tungsten 19600
Uranium 18900
Vanadium 5494
White metal 7100
Wrought Iron 7750
Zinc 7135
Yellow Brass 8470