Optical properties of some commonly used glazing materials

The ideal solar collecting energy glazing material is transparent to short-wave infrared radiation and opaque to long-wave radiation.

Typical optical properties of some common glazing materials are indicated below:

Material Thickness
(mm)
Short-wave Infrared Solar Transmittance Long-Wave Infrared Transmittance
Window glass (float glass) 4 0.83 0.02
Low-iron glass 3 0.89 0.08
Acrylic Glass - Poly(methyl methacrylate) (common trade names Plexiglas, Limacryl, R-Cast, Perspex, Plazcryl, Acrylex, Acrylite, Acrylplast, Altuglas, Polycast, Oroglass and Lucite) 3 0.82 0.02
Polyvinyl Fluoride (known by his trade name Tedlar from DuPont) 0.1 0.92 0.22
Polyester, Mylar 0.1 0.87 0.18

 