Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!

Engineering ToolBox > PE Pipes and Weights

Weight of PE pipes

Approximately weights of polyethylene high density - PEH - pipes:

Outside Diameter
(mm)
Pressure Rating
PN 2.5 PN 4 PN 6 PN 10 PN 16
Pipe Weight (kg/m)
20       0.11 0.16
25     0.13 0.17 0.24
32     0.19 0.28 0.39
40   0.21 0.29 0.44 0.61
50   0.32 0.45 0.68 0.95
63 0.33 0.48 0.70 1.1 1.5
75 0.46 0.69 0.9 1.5 2.1
90 0.65 0.99 1.4 2.2 3.1
110 0.96 1.5 2.1 3.2 4.6
125 1.3 1.9 2.7 4.1 5.9
140 1.6 2.4 3.4 5.2 7.8
160 2.0 3.1 4.4 6.8 9.6
180 2.5 3.9 5.6 8.6 12.1
200 3.1 4.8 6.9 10.6 15.0
225 3.9 6.0 8.7 13.4 19.0
250 4.9 7.4 10.7 16.4 23.4
280 6.1 9.2 13.4 20.6 29
315 7.6 11.8 17.0 26.0 37
355 9.7 14.9 21.6 33.0 47
400 12.3 18.8 27.3 41.9 60
450 15.9 24.3 35.3 54.3 77
500 19.7 30.0 43.0 67  
560 24.5 37.7 54.5 84  
600 26.9 43.7 63 96  
630 31.0 47.7 69 106  
710 39.5 60.5 88    
800 50 77 111    
900 63 97 141    
1000 78 120 173    
1200 112 172      
1400          
1600 199 306      

PE pipes are produced in different pressure grades - PN grades - indicating the pressure in bars the pipe can support with water at 20 oC.

The pressure grades available according to European standards are

Related Topics