Dimensions of Schedule 5 Carbon Steel Pipe or Type 304/304L and Type 316/316L Stainless steel pipe are indicated in the table below:

Nominal Diameter Actual Outside Diameter Inside Diameter Wall Thickness Weight
(inches) (mm) (inches) (mm) (inches) (mm) (inches) (mm) (lbs/ft) (kg/m)
1/2 15 0.840 21.3 0.710 18.0 0.065 1.7 0.6 0.9
3/4 20 1.050 26.9 0.920 23.4 0.065 1.7 0.7 1.1
1 25 1.315 33.7 1.185 30.1 0.065 1.7 0.9 1.3
1 1/4 32 1.660 42.4 1.530 38.9 0.065 1.7 1.1 1.6
1 1/2 40 1.900 48.3 1.770 45.0 0.065 1.7 1.3 1.9
2 50 2.375 60.3 2.2245 57.0 0.065 1.7 1.6 2.4