Resources, Tools and Basic Information for Engineering and Design of Technical Applications!
mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!
Engineering ToolBox > Friction Loss Pressfit Pipes
The tables below indicates friction loss for water flow through pressfit pipes Schedule 5 Carbon Steel Pipe or Type 304/304L and Type 316/316L Stainless steel pipe.
The pressure drop calculations are made with the D'Arcy-Weisbach Equation.
| Flow | Velocity | Pressure Drop | ||||||
| (m3/s) | (liter/s) | (US gpm) | (m/s) | (ft/s) | (Pa/100m) | (mmH2O/100m) | (psi/100ft) | (ftH2O/100ft) |
| 4.0E-5 | 0.04 | 0.63 | 0.157 | 0.52 | 3289 | 335 | 0.145 | 0.34 |
| 5.0E-5 | 0.05 | 0.79 | 0.196 | 0.64 | 4818 | 491 | 0.21 | 0.49 |
| 6.0E-5 | 0.06 | 0.95 | 0.24 | 0.77 | 6629 | 676 | 0.29 | 0.68 |
| 7.0E-5 | 0.07 | 1.11 | 0.28 | 0.9 | 8813 | 899 | 0.39 | 0.9 |
| 8.0E-5 | 0.08 | 1.27 | 0.31 | 1.03 | 10963 | 1118 | 0.48 | 1.12 |
| 9.0E-5 | 0.09 | 1.43 | 0.35 | 1.16 | 13528 | 1379 | 0.6 | 1.38 |
| 1.0E-4 | 0.1 | 1.59 | 0.39 | 1.29 | 16701 | 1703 | 0.74 | 1.7 |
| 1.1E-4 | 0.11 | 1.74 | 0.43 | 1.42 | 19691 | 2008 | 0.87 | 2.0 |
| 1.2E-4 | 0.12 | 1.9 | 0.47 | 1.55 | 22817 | 2327 | 1.01 | 2.3 |
| 1.3E-4 | 0.13 | 2.1 | 0.51 | 1.68 | 26778 | 2731 | 1.18 | 2.7 |
| 1.4E-4 | 0.14 | 2.2 | 0.55 | 1.8 | 30217 | 3081 | 1.34 | 3.1 |
| 1.5E-4 | 0.15 | 2.4 | 0.59 | 1.93 | 34688 | 3537 | 1.53 | 3.5 |
| 1.6E-4 | 0.16 | 2.5 | 0.63 | 2.1 | 38370 | 3913 | 1.7 | 3.9 |
| 1.7E-4 | 0.17 | 2.7 | 0.67 | 2.2 | 43317 | 4417 | 1.91 | 4.4 |
| 1.8E-4 | 0.18 | 2.9 | 0.71 | 2.3 | 47175 | 4810 | 2.1 | 4.8 |
| 1.9E-4 | 0.19 | 3.0 | 0.75 | 2.4 | 52562 | 5360 | 2.3 | 5.4 |
| 2.0E-4 | 0.2 | 3.2 | 0.79 | 2.6 | 58241 | 5939 | 2.6 | 5.9 |
| 3.0E-4 | 0.3 | 4.8 | 1.18 | 3.9 | 123334 | 12576 | 5.5 | 12.6 |
| Flow | Velocity | Pressure Drop | ||||||
| (m3/s) | (liter/s) | (US gpm) | (m/s) | (ft/s) | (Pa/100m) | (mmH2O/100m) | (psi/100ft) | (ftH2O/100ft) |
| 5.0E-5 | 0.05 | 0.79 | 0.12 | 0.39 | 1509 | 154 | 0.067 | 0.154 |
| 6.0E-5 | 0.06 | 0.95 | 0.144 | 0.47 | 2082 | 212 | 0.092 | 0.21 |
| 7.0E-5 | 0.07 | 1.11 | 0.168 | 0.55 | 2711 | 276 | 0.12 | 0.28 |
| 8.0E-5 | 0.08 | 1.27 | 0.193 | 0.63 | 3379 | 345 | 0.149 | 0.34 |
| 9.0E-5 | 0.09 | 1.43 | 0.22 | 0.71 | 4175 | 426 | 0.185 | 0.43 |
| 1.0E-4 | 0.1 | 1.59 | 0.24 | 0.79 | 5029 | 513 | 0.22 | 0.51 |
| 1.1E-4 | 0.11 | 1.74 | 0.26 | 0.87 | 5933 | 605 | 0.26 | 0.61 |
| 1.2E-4 | 0.12 | 1.9 | 0.29 | 0.95 | 6880 | 702 | 0.3 | 0.7 |
| 1.3E-4 | 0.13 | 2.1 | 0.31 | 1.03 | 8074 | 823 | 0.36 | 0.82 |
| 1.4E-4 | 0.14 | 2.2 | 0.34 | 1.11 | 9117 | 930 | 0.4 | 0.93 |
| 1.5E-4 | 0.15 | 2.4 | 0.36 | 1.18 | 10466 | 1067 | 0.46 | 1.07 |
| 1.6E-4 | 0.16 | 2.5 | 0.39 | 1.26 | 11587 | 1181 | 0.51 | 1.18 |
| 1.7E-4 | 0.17 | 2.7 | 0.41 | 1.34 | 13080 | 1334 | 0.58 | 1.34 |
| 1.8E-4 | 0.18 | 2.9 | 0.43 | 1.42 | 14257 | 1454 | 0.63 | 1.46 |
| 1.9E-4 | 0.19 | 3.0 | 0.46 | 1.5 | 15885 | 1620 | 0.7 | 1.62 |
| 2.0E-4 | 0.2 | 3.2 | 0.48 | 1.58 | 17601 | 1795 | 0.78 | 1.8 |
| 3.0E-4 | 0.3 | 4.8 | 0.72 | 2.4 | 36208 | 3692 | 1.6 | 3.7 |
| 4.0E-4 | 0.4 | 6.3 | 0.96 | 3.2 | 62358 | 6359 | 2.8 | 6.4 |
| 5.0E-4 | 0.5 | 7.9 | 1.2 | 3.9 | 94292 | 9615 | 4.2 | 9.6 |
| 6.0E-4 | 0.6 | 9.5 | 1.44 | 4.7 | 131254 | 13384 | 5.8 | 13.4 |
| 7.0E-4 | 0.7 | 11.1 | 1.68 | 5.5 | 178651 | 18217 | 7.9 | 18.2 |
| Flow | Velocity | Pressure Drop | ||||||
| (m3/s) | (liter/s) | (US gpm) | (m/s) | (ft/s) | (Pa/100m) | (mmH2O/100m) | (psi/100ft) | (ftH2O/100ft) |
| 9.0E-5 | 0.09 | 1.43 | 0.127 | 0.42 | 1160 | 118 | 0.051 | 0.118 |
| 1.0E-4 | 0.1 | 1.59 | 0.141 | 0.46 | 1399 | 143 | 0.062 | 0.143 |
| 1.1E-4 | 0.11 | 1.74 | 0.156 | 0.51 | 1652 | 168 | 0.073 | 0.169 |
| 1.2E-4 | 0.12 | 1.9 | 0.17 | 0.56 | 1918 | 196 | 0.085 | 0.196 |
| 1.3E-4 | 0.13 | 2.1 | 0.184 | 0.6 | 2251 | 230 | 0.099 | 0.23 |
| 1.4E-4 | 0.14 | 2.2 | 0.198 | 0.65 | 2545 | 260 | 0.113 | 0.26 |
| 1.5E-4 | 0.15 | 2.4 | 0.21 | 0.7 | 2847 | 290 | 0.126 | 0.29 |
| 1.6E-4 | 0.16 | 2.5 | 0.23 | 0.74 | 3239 | 330 | 0.143 | 0.33 |
| 1.7E-4 | 0.17 | 2.7 | 0.24 | 0.79 | 3561 | 363 | 0.157 | 0.36 |
| 1.8E-4 | 0.18 | 2.9 | 0.25 | 0.84 | 3992 | 407 | 0.176 | 0.41 |
| 1.9E-4 | 0.19 | 3.0 | 0.27 | 0.88 | 4328 | 441 | 0.191 | 0.44 |
| 2.0E-4 | 0.2 | 3.2 | 0.28 | 0.93 | 4795 | 489 | 0.21 | 0.49 |
| 3.0E-4 | 0.3 | 4.8 | 0.42 | 1.39 | 9890 | 1008 | 0.44 | 1.01 |
| 4.0E-4 | 0.4 | 6.3 | 0.57 | 1.86 | 16517 | 1684 | 0.73 | 1.69 |
| 5.0E-4 | 0.5 | 7.9 | 0.71 | 2.3 | 24975 | 2547 | 1.1 | 2.5 |
| 6.0E-4 | 0.6 | 9.5 | 0.85 | 2.8 | 34765 | 3545 | 1.54 | 3.5 |
| 7.0E-4 | 0.7 | 11.1 | 0.99 | 3.2 | 47319 | 4825 | 2.1 | 4.8 |
| 8.0E-4 | 0.8 | 12.7 | 1.13 | 3.7 | 59674 | 6085 | 2.6 | 6.1 |
| 9.0E-4 | 0.9 | 14.3 | 1.27 | 4.2 | 75525 | 7701 | 3.3 | 7.7 |
| 0.0010 | 1.0 | 15.9 | 1.41 | 4.6 | 89910 | 9168 | 4.0 | 9.2 |
| 0.0011 | 1.1 | 17.4 | 1.56 | 5.1 | 108791 | 11093 | 4.8 | 11.1 |
| 0.0012 | 1.2 | 19.0 | 1.7 | 5.6 | 129471 | 13202 | 5.7 | 13.2 |
| 0.0013 | 1.3 | 21 | 1.84 | 6.0 | 151948 | 15494 | 6.7 | 15.5 |
| 0.0014 | 1.4 | 22 | 1.98 | 6.5 | 169697 | 17304 | 7.5 | 17.3 |
| 0.0015 | 1.5 | 24 | 2.1 | 7.0 | 194805 | 19864 | 8.6 | 19.9 |
| Flow | Velocity | Pressure Drop | ||||||
| (m3/s) | (liter/s) | (US gpm) | (m/s) | (ft/s) | (Pa/100m) | (mmH2O/100m) | (psi/100ft) | (ftH2O/100ft) |
| 1.7E-4 | 0.17 | 2.7 | 0.142 | 0.47 | 1011 | 103 | 0.045 | 0.103 |
| 1.8E-4 | 0.18 | 2.9 | 0.151 | 0.49 | 1133 | 116 | 0.05 | 0.116 |
| 1.9E-4 | 0.19 | 3.0 | 0.159 | 0.52 | 1230 | 125 | 0.054 | 0.126 |
| 2.0E-4 | 0.2 | 3.2 | 0.167 | 0.55 | 1363 | 139 | 0.06 | 0.139 |
| 3.0E-4 | 0.3 | 4.8 | 0.25 | 0.82 | 2744 | 280 | 0.121 | 0.28 |
| 4.0E-4 | 0.4 | 6.3 | 0.33 | 1.1 | 4592 | 468 | 0.2 | 0.47 |
| 5.0E-4 | 0.5 | 7.9 | 0.42 | 1.37 | 6951 | 709 | 0.31 | 0.71 |
| 6.0E-4 | 0.6 | 9.5 | 0.5 | 1.65 | 9686 | 988 | 0.43 | 0.99 |
| 7.0E-4 | 0.7 | 11.1 | 0.59 | 1.92 | 12744 | 1300 | 0.56 | 1.3 |
| 8.0E-4 | 0.8 | 12.7 | 0.67 | 2.2 | 16072 | 1639 | 0.71 | 1.64 |
| 9.0E-4 | 0.9 | 14.3 | 0.75 | 2.5 | 20341 | 2074 | 0.9 | 2.1 |
| 0.0010 | 1.0 | 15.9 | 0.84 | 2.7 | 24215 | 2469 | 1.07 | 2.5 |
| 0.0011 | 1.1 | 17.4 | 0.92 | 3.0 | 29301 | 2988 | 1.29 | 3.0 |
| 0.0012 | 1.2 | 19.0 | 1.0 | 3.3 | 34870 | 3556 | 1.54 | 3.6 |
| 0.0013 | 1.3 | 21 | 1.09 | 3.6 | 39408 | 4018 | 1.74 | 4.0 |
| 0.0014 | 1.4 | 22 | 1.17 | 3.8 | 45704 | 4660 | 2.0 | 4.7 |
| 0.0015 | 1.5 | 24 | 1.26 | 4.1 | 52467 | 5350 | 2.3 | 5.4 |
| 0.0016 | 1.6 | 25 | 1.34 | 4.4 | 59695 | 6087 | 2.6 | 6.1 |
| 0.0017 | 1.7 | 27 | 1.42 | 4.7 | 67391 | 6872 | 3.0 | 6.9 |
| 0.0018 | 1.8 | 29 | 1.51 | 4.9 | 72646 | 7408 | 3.2 | 7.4 |
| 0.0019 | 1.9 | 30 | 1.59 | 5.2 | 80942 | 8254 | 3.6 | 8.3 |
| 0.0020 | 2.0 | 32 | 1.67 | 5.5 | 89687 | 9145 | 4.0 | 9.2 |
| 0.0030 | 3.0 | 48 | 2.5 | 8.2 | 193723 | 19754 | 8.6 | 19.8 |
| Flow | Velocity | Pressure Drop | ||||||
| (m3/s) | (liter/s) | (US gpm) | (m/s) | (ft/s) | (Pa/100m) | (mmH2O/100m) | (psi/100ft) | (ftH2O/100ft) |
| 3.0E-4 | 0.3 | 4.8 | 0.189 | 0.62 | 1381 | 141 | 0.061 | 0.141 |
| 4.0E-4 | 0.4 | 6.3 | 0.25 | 0.83 | 2315 | 236 | 0.102 | 0.24 |
| 5.0E-4 | 0.5 | 7.9 | 0.31 | 1.03 | 3508 | 358 | 0.155 | 0.36 |
| 6.0E-4 | 0.6 | 9.5 | 0.38 | 1.24 | 4736 | 483 | 0.21 | 0.48 |
| 7.0E-4 | 0.7 | 11.1 | 0.44 | 1.44 | 6446 | 657 | 0.28 | 0.66 |
| 8.0E-4 | 0.8 | 12.7 | 0.5 | 1.65 | 8139 | 830 | 0.36 | 0.83 |
| 9.0E-4 | 0.9 | 14.3 | 0.57 | 1.86 | 9946 | 1014 | 0.44 | 1.02 |
| 0.0010 | 1.0 | 15.9 | 0.63 | 2.1 | 12279 | 1252 | 0.54 | 1.25 |
| 0.0011 | 1.1 | 17.4 | 0.69 | 2.3 | 14326 | 1461 | 0.63 | 1.46 |
| 0.0012 | 1.2 | 19.0 | 0.75 | 2.5 | 17050 | 1739 | 0.75 | 1.74 |
| 0.0013 | 1.3 | 21 | 0.82 | 2.7 | 20010 | 2040 | 0.88 | 2.0 |
| 0.0014 | 1.4 | 22 | 0.88 | 2.9 | 22347 | 2279 | 0.99 | 2.3 |
| 0.0015 | 1.5 | 24 | 0.94 | 3.1 | 25653 | 2616 | 1.13 | 2.6 |
| 0.0016 | 1.6 | 25 | 1.01 | 3.3 | 29188 | 2976 | 1.29 | 3.0 |
| 0.0017 | 1.7 | 27 | 1.07 | 3.5 | 32950 | 3360 | 1.46 | 3.4 |
| 0.0018 | 1.8 | 29 | 1.13 | 3.7 | 35520 | 3622 | 1.57 | 3.6 |
| 0.0019 | 1.9 | 30 | 1.19 | 3.9 | 39576 | 4036 | 1.75 | 4.0 |
| 0.0020 | 2.0 | 32 | 1.26 | 4.1 | 43852 | 4472 | 1.94 | 4.5 |
| 0.0030 | 3.0 | 48 | 1.89 | 6.2 | 94720 | 9659 | 4.2 | 9.7 |
| 0.0040 | 4.0 | 63 | 2.5 | 8.3 | 161375 | 16455 | 7.1 | 16.5 |
| Flow | Velocity | Pressure Drop | ||||||
| (m3/s) | (liter/s) | (US gpm) | (m/s) | (ft/s) | (Pa/100m) | (mmH2O/100m) | (psi/100ft) | (ftH2O/100ft) |
| 5.0E-4 | 0.5 | 7.9 | 0.196 | 0.64 | 1110 | 113 | 0.049 | 0.113 |
| 6.0E-4 | 0.6 | 9.5 | 0.24 | 0.77 | 1549 | 158 | 0.068 | 0.158 |
| 7.0E-4 | 0.7 | 11.1 | 0.27 | 0.9 | 2043 | 208 | 0.09 | 0.21 |
| 8.0E-4 | 0.8 | 12.7 | 0.31 | 1.03 | 2582 | 263 | 0.114 | 0.26 |
| 9.0E-4 | 0.9 | 14.3 | 0.35 | 1.16 | 3159 | 322 | 0.14 | 0.32 |
| 0.0010 | 1.0 | 15.9 | 0.39 | 1.29 | 3766 | 384 | 0.166 | 0.38 |
| 0.0011 | 1.1 | 17.4 | 0.43 | 1.41 | 4556 | 465 | 0.2 | 0.47 |
| 0.0012 | 1.2 | 19.0 | 0.47 | 1.54 | 5422 | 553 | 0.24 | 0.55 |
| 0.0013 | 1.3 | 21 | 0.51 | 1.67 | 6137 | 626 | 0.27 | 0.63 |
| 0.0014 | 1.4 | 22 | 0.55 | 1.8 | 7117 | 726 | 0.31 | 0.73 |
| 0.0015 | 1.5 | 24 | 0.59 | 1.93 | 8170 | 833 | 0.36 | 0.83 |
| 0.0016 | 1.6 | 25 | 0.63 | 2.1 | 8951 | 913 | 0.4 | 0.91 |
| 0.0017 | 1.7 | 27 | 0.67 | 2.2 | 10105 | 1030 | 0.45 | 1.03 |
| 0.0018 | 1.8 | 29 | 0.71 | 2.3 | 11329 | 1155 | 0.5 | 1.16 |
| 0.0019 | 1.9 | 30 | 0.74 | 2.4 | 12623 | 1287 | 0.56 | 1.29 |
| 0.0020 | 2.0 | 32 | 0.78 | 2.6 | 13449 | 1371 | 0.59 | 1.37 |
| 0.0030 | 3.0 | 48 | 1.18 | 3.9 | 29049 | 2962 | 1.28 | 3.0 |
| 0.0040 | 4.0 | 63 | 1.57 | 5.1 | 49491 | 5047 | 2.2 | 5.1 |
| 0.0050 | 5.0 | 79 | 1.96 | 6.4 | 77329 | 7885 | 3.4 | 7.9 |
| 0.0060 | 6.0 | 95 | 2.4 | 7.7 | 106513 | 10861 | 4.7 | 10.9 |
| 0.0070 | 7.0 | 111 | 2.7 | 9.0 | 144976 | 14783 | 6.4 | 14.8 |
| 0.0080 | 8.0 | 127 | 3.1 | 10.3 | 189356 | 19309 | 8.4 | 19.3 |
A diagram presentation of the tables above can be found in "Pressfit Pipes - Pressure Loss Diagram".