Engineering ToolBox > Pressure Loss of Water Due to Friction in Copper Tubes
Pressure loss of water due to friction (major loss) in copper pipes, Types K, L and M tubes according ASTM B88, can be found in the diagram and tables below:

The diagram as pdf-file pressure loss copper pipes ASTM B88 - Type K.





The pressure loss is based on the Hazen-Williams formula with roughness coefficient c = 145.