Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!

Engineering ToolBox > PVC and CPVC Pipes - Schedule 40 & 80

Standard dimensions and weight of PVC - Polyvinyl Chloride - and CPVC - Chlorinated Polyvinyl Chloride - pipes according ASTM D1785

Typical weight and dimensions of PVC and CPVC pipes according ASTM D1785 "Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Pipe, Schedules 40, 80, and 120" can be found in the table below:

PVC and CPVC Pipes - Schedule 40
Nominal Pipe Size
(inches)
Outside Diameter
(inches)
Minimum Wall Thickness
(inches)
Nominal Inside Diameter
(inches)
Weight
(lb/100 ft)
PVC CPVC
1/2 0.840 0.109 0.622 16 17
3/4 1.050 0.113 0.824 21 23
1 1.315 0.133 1.049 32 34
1 1/4 1.660 0.140 1.380 43 46
1 1/2 1.900 0.145 1.610 51 55
2 2.375 0.154 2.067 68 74
2 1/2 2.875 0.203 2.469 107 118
3 3.500 0.216 3.068 141 154
4 4.500 0.237 4.026 201 220
5 5.563 0.258 5.047 273
6 6.625 0.280 6.065 353 386
8 8.625 0.322 7.981 539 581
10 10.750 0.365 10.020 755 824
12 12.750 0.406 11.938 1001 1089
14 14.000 0.438 13.124 1180
16 16.000 0.500 15.000 1543

PVC and CPVC Pipes - Schedule 80
Nominal Pipe Size
(inches)
Outside Diameter
(inches)
Minimum Wall Thickness
(inches)
Nominal Inside Diameter
(inches)
Weight
(lb/100 ft)
PVC CPVC
1/2 0.840 0.147 0.546 20 22
3/4 1.050 0.154 0.742 27 30
1 1.315 0.179 0.957 41 44
1 1/4 1.660 0.191 1.278 52 61
1 1/2 1.900 0.200 1.500 67 74
2 2.375 0.218 1.939 95 102
2 1/2 2.875 0.276 2.323 145 156
3 3.500 0.300 2.900 194 209
4 4.500 0.337 3.826 275 305
5 5.563 0.375 4.813 387
6 6.625 0.432 5.761 542 582
8 8.625 0.500 7.625 805 883
10 10.750 0.593 9.564 1200 1309
12 12.750 0.687 11376 1650 180
14 14.000 0.750 12.500 1930
16 16.000 0.843 14.314 2544