| Material | Emissivity Coefficient - ε - |
| Water | 0.993 - 0.998 |
| Ice | 0.98 |
| Snow | 0.969 - 0.997 |
| Sand | 0.949 - 0.962 |
| Granite | 0.898 |
| Green Grass | 0.975 - 0.986 |