Softwood lumber standard applied to boards, dimensional lumber and timber:
| Item | Thickness | Face Widths | ||||
| Nominal | Minimum Dressed | Nominal | Minimum Dressed | |||
| Dry (max 19% moisture content) (inches) | Green (inches) | Dry (max 19% moisture content) (inches) | Green (inches) | |||
| Boards | 2 | 1 1/2 | 1 9/16 | |||
| 3 | 2 1/2 | 2 9/16 | ||||
| 4 | 3 1/2 | 3 9/16 | ||||
| 3/8 | 5/16 | 11/32 | 5 | 4 1/2 | 4 5/8 | |
| 1/2 | 7/16 | 15/32 | 6 | 5 1/2 | 5 5/8 | |
| 5/8 | 9/16 | 19/32 | 7 | 6 1/2 | 6 5/8 | |
| 3/4 | 5/8 | 11/16 | 8 | 7 1/4 | 7 1/2 | |
| 1 | 3/4 | 25/32 | 9 | 8 1/4 | 8 1/2 | |
| 1 1/4 | 1 | 1 1/32 | 10 | 9 1/4 | 9 1/2 | |
| 1 1/2 | 1 1/4 | 1 9/32 | 11 | 10 1/4 | 10 1/2 | |
| 12 | 11 1/4 | 11 1/2 | ||||
| 14 | 13 1/4 | 13 1/2 | ||||
| 16 | 15 1/4 | 15 1/2 | ||||
| Dimension | 2 | 1 1/2 | 1 9/16 | |||
| 2 1/2 | 2 | 2 1/16 | ||||
| 3 | 2 1/2 | 2 9/16 | ||||
| 2 | 1 1/2 | 1 9/16 | 3 1/2 | 3 | 3 1/16 | |
| 2 1/2 | 2 | 2 1/16 | 4 | 3 1/2 | 3 9/16 | |
| 3 | 2 1/2 | 2 9/16 | 4 1/2 | 4 | 4 1/16 | |
| 3 1/2 | 3 | 3 1/16 | 5 | 4 1/2 | 4 5/8 | |
| 4 | 3 1/2 | 3 9/16 | 6 | 5 1/2 | 5 5/8 | |
| 4 1/2 | 4 | 4 1/16 | 8 | 7 1/4 | 7 1/2 | |
| 10 | 9 1/4 | 9 1/2 | ||||
| 12 | 11 1/4 | 11 1/2 | ||||
| 14 | 13 1/4 | 13 1/2 | ||||
| 16 | 15 1/4 | 15 1/2 | ||||
| Timbers | 5 & 6 thick | 1/2 off | 1/2 off | 5 & 6 wide | 1/2 off | 1/2 off |
| 7 - 15 thick | 3/4 off | 1/2 off | 7 - 15 wide | 3/4 off | 1/2 off | |
| >= 16 thick | 1 off | 1/2 off | >= 16 wide | 1 off | 1/2 off | |