Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

mobile - visible on handheld devices - alternatively go to www.engineeringtoolbox.com!

Engineering ToolBox > Speed of Sound in some common Solids

Velocity of sound in some common solids as aluminum, brass, concrete and ...

Speed of sound in normal air is 343 m/s. In water the speed is 1,433 m/s. The sound velocity in some common solids can be found from the table below.

Medium Velocity

(m/s)
(ft/s)
Aluminum 4877 16000
Brass 3475 11400
Brick 4176 13700
Concrete 3200 - 3600 10500 - 11800
Copper 3901 12800
Cork 366 - 518 1200 - 1700
Diamond 12000 39400
Glass 3962 13000
Glass, Pyrex 5640 18500
Gold 3240 10630
Hardwood 3962 13000
Iron 5130 16830
Lead 1158 3800
Lucite 2680 8790
Rubber 40 - 150 130 - 492
Steel 6100 20000
Water 1433 4700
Wood (hard) 3960 13000
Wood 3300 - 3600 10820 - 11810