The specific gravity of some common liquids or fluids can be found in the table below:
| Product | Temperature | Specific Gravity SG 1) | |
| oF | oC | ||
| Acetaldehyde CH3CHO | 61 68 | 16.1 20 | 0.79 0.76 |
| Acetic acid 5% - vinegar | 59 | 15 | 1.006 |
| Acetic acid - 10% | 59 | 15 | 1.014 |
| Acetic acid - 50% | 59 | 15 | 1.061 |
| Acetic acid - 80% | 59 | 15 | 1.075 |
| Acetic acid - concentrated | 59 | 15 | 1.055 |
| Acetic acid anhydride (CH3COO)2O | 59 | 15 | 1.087 |
| Acetone CH3COCH3 | 68 | 20 | 0.792 |
| Alcohol - allyl | 68 | 20 | 0.855 |
| Alcohol - butyl-n | 68 158 | 20 70 | 0.81 0.78 |
| Alcohol - ethyl (grain) C2H5OH | 68 104 | 20 40 | 0.789 0.772 |
| Alcohol - methyl (wood) CH3OH | 68 | 20 | 0.79 |
| Alcohol - propyl | 68 32 | 20 0 | 0.804 0.817 |
| Aluminum sulfate 36% solution | 60 | 15.6 | 1.055 |
| Ammonia | 0 | -17.8 | 0.662 |
| Aniline | 68 32 | 20 0 | 1.022 1.035 |
| Automotive crankcase oils SAE-5W/10W/20W/30W/40W/50W | 60 | 15.6 | 0.88-0.94 |
| Automotive gear oils SAE-75W/80W/85W/90W/140W/150W | 60 | 15.6 | 0.88-0.94 |
| Beer | 60 | 15.6 | 1.01 |
| Benzene (benzol) C6H6 | 32 60 | 0 15.6 | 0.899 0.885 |
| Bone oil | 60 | 15.6 | 0.918 |
| Boric acid H3BO3 | 46.4 59 | 8 15 | 1.014 1.025 |
| Bromine | 32 | 0 | 2.9 |
| Butane-n | 60 | 15.6 | 0.584 |
| Butyric acid | 68 | 20 | 0.959 |
| Calcium chloride 5% | 65 | 18.3 | 1.040 |
| Calcium chloride 25% | 60 | 15.6 | 1.23 |
| Carbolic acid (phenol) | 65 | 18.3 | 1.08 |
| Carbon tetrachloride CCl4 | 68 | 20 | 1.594 |
| Carbon disulfide CS2 | 32 68 | 0 20 | 1.293 1.263 |
| Castor Oil | 68 104 | 20 40 | 0.96 0.95 |
| China wood oil | 60 | 15.6 | 0.943 |
| Chloroform | 68 140 | 20 60 | 1.489 1.413 |
| Coconut oil | 60 | 15.6 | 0.925 |
| Cod liver oil | 59 | 15 | 0.920-0.925 |
| Corn oil | 60 | 15.6 | 0.924 |
| Cotton seed oil | 60 | 15.6 | 0.88-0.93 |
| Creosote | 60 | 15.6 | 1.04-1.10 |
| Crude oil 48o API | 60 130 | 15.6 54.4 | 0.79 0.76 |
| Crude oil 40o API | 60 130 | 15.6 54.4 | 0.825 0.805 |
| Crude oil 35.6o API | 60 130 | 15.6 54.4 | 0.847 0.824 |
| Crude oil 32.6o API | 60 130 | 15.6 54.4 | 0.832 0.84 |
| Crude oil Salt creek | 60 130 | 15.6 54.4 | 0.843 0.82 |
| Decane-n | 68 | 20 | 0.73 |
| Diethylene glycol | 60 | 15.6 | 1.12 |
| Diethyl ether | 68 | 20 | 0.714 |
| Diphenylamine | 1.16 | ||
| Diesel Fuel Oil 2D/3D/4D/5D | 60 | 15.6 | 0.81 - 0.96 |
| Dowtherm | 77 | 25 | 1.056 |
| Ethyl acetate CH3COOC2H3 | 59 68 | 15 20 | 0.907 0.90 |
| Ethyl bromide C2H3Br | 59 | 15 | 1.45 |
| Ethylene bromide | 68 | 20 | 2.18 |
| Ethylene chloride | 68 | 20 | 1.246 |
| Ethylene glycol | 60 | 15.6 | 1.125 |
| Formic acid - 10% | 68 | 20 | 1.025 |
| Formic acid - 50% | 68 | 20 | 1.121 |
| Formic acid - 80% | 68 | 20 | 1.186 |
| Formic acid - concentrated | 68 | 20 | 1.221 |
| Freon - 11 | 70 | 21.1 | 1.49 |
| Freon - 12 | 70 | 21.1 | 1.33 |
| Freon - 21 | 70 | 21.1 | 1.37 |
| Furfurol | 68 | 20 | 1.159 |
| Fuel oils 1/2/3/5A/5B/6 | 60 | 15.6 | 0.82-0.95 |
| Gas oils | 60 | 15.6 | 0.89 |
| Gasoline a | 60 | 15.6 | 0.74 |
| Gasoline b | 60 | 15.6 | 0.72 |
| Gasoline c | 60 | 15.6 | 0.68 |
| Glycerin 100% | 68 | 20 | 1.26 |
| Glycerin 50% water | 68 | 20 | 1.13 |
| Glucose | 60 | 15.6 | 1.35-1.44 |
| Heptane-n | 60 | 15.6 | 0.688 |
| Hexane-n | 60 | 15.6 | 0.664 |
| Ink printers | 60 | 15.6 | 1.0-1.4 |
| Kerosene | 60 | 15.6 | 0.78-0.82 |
| Jet fuel | 60 | 15.6 | 0.82 |
| Lard | 60 | 15.6 | 0.96 |
| Lard oil | 60 | 15.6 | 0.91-0.93 |
| Linseed oil | 60 | 15.6 | 0.92-0.94 |
| Mercury | 60 | 15.6 | 13.6 |
| Methyl acetate | 68 | 20 | 0.93 |
| Methyl iodide | 68 | 20 | 2.28 |
| Milk | 60 | 15.6 | 1.02-1.05 |
| Molasses A first | 60 | 15.6 | 1.40-1.46 |
| Molasses B second | 60 | 15.6 | 1.43-1.48 |
| Molasses C blackstrap | 60 | 15.6 | 1.46-1.49 |
| Naphthalene | 68 | 20 | 1.145 |
| Neatsfoot oil | 60 | 15.6 | 0.917 |
| Nitrobentzene | 68 59 | 20 15 | 1.203 1.205 |
| Nonane-n | 60 68 | 15.6 20 | 0.722 0.718 |
| Octane-n | 60 | 15.6 | 0.707 |
| Olive oil | 60 | 15.6 | 0.91 - 0.92 |
| Palm oil | 60 | 15.6 | 0.924 |
| Peanut oil | 60 | 15.6 | 0.92 |
| Pentane-n | 32 60 | 0 15.6 | 0.650 0.631 |
| Potassium hydrate | 1.24 | ||
| Sodium chloride | 1.19 | ||
| Sodium hydrate | 1.27 | ||
| Tuluol | 0.87 | ||
| Turpentine | 0.87 | ||
| Water. fresh | 1 | ||
| Water. sea 36 oF | 1.02 | ||
| Xylene | 0.87 | ||
1) Based on water at 60oF and SG = 1