| Size (mm x mm) | Dimensions | Static Parameters | |||
| Depth h (mm) | Thickness s (mm) | Sectional Area (cm2) | Weight (kg/m) | Moment of Inertia Ix (cm4) | |
| 25 x 25 | 25 | 5 | 2.26 | 1.77 | 1.20 |
| 25 | 4 | 1.85 | 1.45 | 1.01 | |
| 25 | 3 | 1.42 | 1.11 | 0.80 | |
| 30 x 30 | 30 | 6 | 3.27 | 2.57 | 2.50 |
| 30 | 5 | 2.78 | 2.18 | 2.16 | |
| 40 x 40 | 40 | 5 | 4.48 | 3.52 | 6.31 |
| 40 | 5 | 3.79 | 2.97 | 4.53 | |
| 40 | 4 | 3.08 | 2.42 | 4.47 | |
| 45 x 45 | 45 | 6 | 5.09 | 4.00 | 9.16 |
| 45 | 5 | 4.30 | 3.38 | 7.84 | |
| 45 | 4 | 3.49 | 2.74 | 6.43 | |
| 50 x 50 | 50 | 8 | 7.41 | 5.82 | 16.3 |
| 50 | 6 | 5.69 | 4.47 | 12.8 | |
| 50 | 5 | 4.8 | 3.77 | 11.0 | |
| 60 x 60 | 60 | 10 | 11.1 | 8.69 | 34.9 |
| 60 | 8 | 9.03 | 7.09 | 29.2 | |
| 60 | 6 | 6.91 | 5.42 | 22.8 | |
| 60 | 5 | 5.82 | 4.57 | 19.4 | |
| 70 x 70 | 70 | 10 | 13.1 | 10.3 | 57.2 |
| 70 | 8 | 10.6 | 8.36 | 47.5 | |
| 70 | 6 | 8.1 | 6.38 | 36.9 | |
| 80 x 80 | 80 | 10 | 15.1 | 11.8 | 87.5 |
| 80 | 8 | 12.3 | 9.63 | 72.2 | |
| 80 | 6 | 9.25 | 7.34 | 55.8 | |
| 90 x 90 | 90 | 12 | 20.3 | 15.9 | 148 |
| 90 | 10 | 17.1 | 13.4 | 127 | |
| 90 | 8 | 13.9 | 10.9 | 104 | |
| 90 | 6 | 10.6 | 8.3 | 80.3 | |
| 100 x 100 | 100 | 15 | 27.9 | 21.9 | 204 |
| 100 | 12 | 22.7 | 17.8 | 207 | |
| 100 | 10 | 19.2 | 15.0 | 118 | |
| 100 | 8 | 15.5 | 12.2 | 145 | |
| 120 x 120 | 120 | 15 | 33.9 | 26.6 | 445 |
| 120 | 12 | 27.5 | 21.6 | 368 | |
| 120 | 10 | 23.2 | 18.2 | 313 | |
| 120 | 8 | 18.7 | 14.7 | 255 | |
| 150 x 150 | 150 | 18 | 51.0 | 40.1 | 1050 |
| 150 | 15 | 43.0 | 33.8 | 898 | |
| 150 | 12 | 34.8 | 27.3 | 737 | |
| 150 | 10 | 29.3 | 23.0 | 624 | |
| 200 x 200 | 200 | 24 | 90.6 | 71.1 | 3330 |
| 200 | 20 | 76.3 | 59.9 | 2850 | |
| 200 | 18 | 69.1 | 54.2 | 2600 | |
| 200 | 16 | 61.8 | 48.5 | 2340 | |