Thermal properties of Sulfur Dioxide SO2
| Temperature - t - (oC) |
Density - ρ - (kg/m3) |
Specific Heat - cp - (kJ/kg K) |
Thermal Coductivity - λ - (W/m K) |
Dynamic Viscosity 10-6 - η - (Pa s) |
Prandtl's no. |
| 0 | 1435 |
1.33 |
0.212 | 367 |
2.31 |
| 20 | 1383 | 1.37 | 0.199 | 304 | 2.09 |
| 50 | 1296 | 1.48 | 0.177 | 234 | 1.96 |