| PVC - Wall Schedule 40 - Support Spacing (feet) | |||
| NPS (inches) | Operating Temperature (oF) | ||
| 60 | 100 | 140 | |
| 1/2 | 4 1/2 | 4 | 2 1/2 |
| 3/4 | 5 | 4 | 2 1/2 |
| 1 | 5 1/2 | 4 1/2 | 2 1/2 |
| 1 1/4 | 5 1/2 | 5 | 3 |
| 1 1/2 | 6 | 5 | 3 |
| 2 | 6 | 5 | 3 |
| 3 | 7 | 6 | 3 1/2 |
| 4 | 7 1/2 | 6 1/2 | 4 |
| 6 | 8 1/2 | 7 1/2 | 4 1/2 |
| 8 | 9 | 8 | 4 1/2 |
| PVC - Wall Schedule 80 - Support Spacing (feet) | |||
| NPS (inches) | Operating Temperature (oF) | ||
| 60 | 100 | 140 | |
| 1/2 | 5 | 4 1/2 | 2 1/2 |
| 3/4 | 5 1/2 | 4 1/2 | 2 1/2 |
| 1 | 6 | 5 | 3 |
| 1 1/2 | 6 1/2 | 5 1/2 | 3 1/2 |
| 2 | 7 | 6 | 3 1/2 |
| 3 | 8 | 7 | 4 |
| 4 | 9 | 7 1/2 | 4 1/2 |
| 6 | 10 | 9 | 5 |
| 8 | 11 | 9 1/2 | 5 1/2 |