Maximum support spacing for epoxy fiberglass pipes at different operating temperatures can be found in the table below. Maximum operating temperature for epoxy pipes should not exceed 300oF (149oC).
| Nominal Pipe Size | Temperature | ||||||||||||
| (oC) | (oF) | (oC) | (oF) | (oC) | (oF) | (oC) | (oF) | (oC) | (oF) | (oC) | (oF) | ||
| 24 | 75 | 66 | 150 | 79 | 175 | 93 | 200 | 107 | 225 | 121 | 250 | ||
| Maximum Support Spacing | |||||||||||||
| (inches) | (mm) | (m) | (ft) | (m) | (ft) | (m) | (ft) | (m) | (ft) | (m) | (ft) | (m) | (ft) |
| 1 | 25 | 3.2 | 9.9 | 3.0 | 9.8 | 3.0 | 9.7 | 2.9 | 9.4 | 2.8 | 9.3 | 2.7 | 8.7 |
| 1 1/2 | 40 | 3.5 | 11.6 | 3.5 | 11.4 | 3.4 | 11.3 | 3.4 | 11.0 | 3.3 | 10.8 | 3.1 | 10.1 |
| 2 | 50 | 4.0 | 13.1 | 3.9 | 12.9 | 3.9 | 12.8 | 3.8 | 12.4 | 3.7 | 12.2 | 3.5 | 11.4 |
| 3 | 80 | 4.6 | 15.0 | 4.5 | 14.8 | 4.5 | 14.6 | 4.3 | 14.2 | 4.3 | 14.0 | 4.0 | 13.0 |
| 4 | 100 | 5.1 | 16.7 | 5.0 | 16.5 | 5.0 | 16.3 | 4.8 | 15.8 | 4.8 | 15.6 | 4.4 | 14.5 |
| 6 | 150 | 5.8 | 18.9 | 5.7 | 18.6 | 5.6 | 18.4 | 5.5 | 17.9 | 5.4 | 17.6 | 5 | 16.4 |
| 8 | 200 | 6.1 | 20.0 | 6.1 | 20.0 | 6.0 | 19.8 | 5.9 | 19.3 | 5.8 | 19.0 | 5.4 | 17.7 |
| 10 | 250 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 5.7 | 18.8 |
| 12 | 300 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.0 | 19.7 |
| 14 | 350 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 | 6.1 | 20.0 |