Maximum support spacing for PP - PolyPropylene - pipes depends on the operating temperature. Maximum spacing between supports at different temperatures can be found in the tables below:

PP - Wall Schedule 40 - Support Spacing (feet)
NPS
(inches)
Operating Temperature (oF)
60 100 140 180
1/2 1 1/2 1 1/2 1 1/2 1
3/4 2 2 1 1/2 1 1/2
1 2 2 2 1 1/2
1 1/4 2 1/2 2 2 2
1 1/2 2 1/2 2 1/2 2 2
2 3 2 1/2 2 1/2 2
3 3 1/2 2 1/2 3 2 1/2
4 4 3 3 1/2 3

PP - Wall Schedule 80 - Support Spacing (feet)
NPS
(inches)
Operating Temperature (oF)
60 100 140 180
1/2 2 2 2 1 1/2
3/4 2 1/2 2 1/2 2 2
1 2 1/2 2 1/2 2 2
1 1/4 3 2 1/2 2 1/2 2 1/2
1 1/2 3 3 2 1/2 2 1/2
2 3 1/2 3 3 2 1/2
3 4 4 3 1/2 3 1/2
4 4 1/2 4 1/2 4 3 1/2