Maximum support spacing for PVDF - PolyVinylidene Fluoride - pipes depends on the operating temperature. Maximum spacing between supports at different temperatures can be found in the tables below:

PVDF - Wall Schedule 40 - Support Spacing (feet)
NPS
(inches)
Operating Temperature (oF)
80 100 1401)
1/2 3 1/2 3 1/2 2
3/4 4 3 1/2 2 1/2
1 4 4 2 1/2
1 1/2 4 1/2 4 1/2 2 1/2
2 4 1/2 4 1/2 2 1/2

PVDF - Wall Schedule 80 - Support Spacing (feet)
NPS
(inches)
Operating Temperature (oF)
80 100 1401)
1/2 4 1/2 4 1/2 2 1/2
3/4 4 1/2 4 1/2 3
1 5 4 1/2 3
1 1/2 5 1/2 5 3
2 5 1/2 5 3

1) For temperatures above 140oF continuous support is needed.