The table below can be used to calculate the expansion of steam pipes at different operating temperatures.
| Production Temperature (oC) | Expansion pr. 100 m Pipe (mm) |
| 66 | 63 |
| 93 | 96 |
| 121 | 136 |
| 149 | 166 |
| 177 | 203 |
| 204 | 246 |
| 232 | 279 |
| 260 | 323 |
To avoid unacceptable stress and damage of the pipe lines - its important to handle the expansion properly.