Engineering ToolBox > Water Content in Products

Water content before and after drying in some common materials as cork, grain, soap, peat, wood and more

The water content in some common materials before and after drying can be found in the table below:

Material Original water content
before drying
%
Final water content
after drying
%
Coal, bituminous 40 - 60 8 - 12
Earth 45 - 50 -
Earth, sandy 20 - 25 -
Grain 17 - 23 10 - 12
Cork 40 - 45 10 - 15
Glue 80 - 90 -
Glue, air dried 15 -
Hides 45 -
Macaroni 30 - 35 11 - 13
Rubber goods 30 - 50 -
Soap 27 - 35 25 - 26
Starch 38 - 45 12 - 14
Starch, air dried 16 - 20 12 - 14
Pasta, macaroni, spaghetti, noodles 30 - 35 11 - 13
Peat 85 - 90 30 - 35
Yarn, washing 40 - 50 -
Wood, green hard 50 10 - 15
Wood, green soft 30 - 50 10 - 15
Wood, air dried hard 17 - 20 10 - 15
Wood, air dried soft 10 - 15 10 - 15