(103 kg/m3) (lb/ft3)
Alder 0.4 - 0.7 26 - 42
Apple 0.65 - 0.85 41 - 52
Ash, white 0.65 - 0.85 40 - 53
Ash, black 0.54 33
Aspen 0.42 26
Balsa 0.11 - 0.14 7 - 9
Bamboo 0.3 - 0.4 19 - 25
Basswood 0.3 - 0.6 20 - 37
Beech 0.7 - 0.9 32 - 56
Birch, British 0.67 42
Blue gum 1 62
Box 0.95 - 1.2 59 - 72
Butternut 0.38 24
Cedar, red 0.38 23
Cherry 0.7 - 0.9 43- 56
Cypress 0.51 32
Dogwood 0.75 47
Douglas Fir 0.53 33
Ebony 1.1 - 1.3 69 - 83
Elm, English 0.55 - 0.6 34 - 37
Elm, Rock 0.82 50
Hickory 0.6 - 0.9 37 - 58
Holly 0.75 47
Juniper 0.55 35
Larch 0.5 - 0.55 31 - 35
Lignum vitae 1.17 - 1.33 73 - 83
Locust 0.65 - 0.7 42 - 44
Logwood 0.9 57
Mahogany, African 0.5 - 0.85 31 - 53
Mahogany, Honduras 0.65 41
Mahogany, Spanish 0.85 53
Maple 0.6 - 0.75 39 - 47
Oak 0.6 - 0.9 37 - 56
Oregon Pine 0.53 33
Parana Pine 0.56 35
Pear 0.6 - 0.7 38 - 45
Pine, pitch 0.8 - 0.85 52 - 53
Pine, white 0.35 - 0.5 22 - 31
Pine, yellow 0.35 - 0.6 23 - 37
Plum 0.65 - 0.8 41 - 49
Poplar 0.35 - 0.5 22 - 31
Redwood, American 0.45 28
Redwood, European 0.51 32
Satinwood 0.95 59
Spruce 0.4 - 0.7 25 - 44
Spruce, Canadian 0.45 28
Spruce, Sitka 0.45 28
Sycamore 0.4 - 0.6 24 - 37
Teak, Indian 0.65 - 0.9 41 - 55
Teak, African 0.98 61
Walnut 0.65 - 0.7 40 - 43
Water gum 1 62
Willow 0.4 - 0.6 24 - 37